16Mo3 equivalent grades: ASTM, EN, JIS, GB, DIN

16Mo3 is molybdenum-alloyed steel for pressure purposes at elevated temperature specified in EN 10028-2. Below, the grades that can replace it — 5 standard systems in all — with the deciding limit named for each one rather than left to be looked up. The full 16Mo3 data sheet carries the composition and mechanical tables.

Last updated

Where a drawing says 16Mo3, 16Mo satisfies it as written, with no concession needed. A204 Gr. A, A204 Gr. B, A335 P1 and 3 more differ by one requirement, which is a line on the order rather than a redesign. Functionally interchangeable, P265GH, 13CrMo4-5, P355GH serve a different route to the same duty — check the design, not the analysis. The table holds 1 in GB/T (China), 4 in ASTM / ASME, 1 in GOST (Russia/CIS), 1 in JIS (Japan), 3 in EN (European).

Cross-reference table

16Mo3 equivalents by system
GradeSystemMatchWhy / differences
16MoGB/T (China)IdenticalGB/T 713 16Mo (formerly 16MnMoR-type usage); GB adopted the EN name for Mo pressure plate.
A204 Gr. AASTM / ASMENearASTM/ASME A204 Grade A (SA-204-A): C ≤ 0.18, Mo 0.45–0.60, yield 255 MPa, Rm 450–585 MPa. Higher Mo than 16Mo3; Grade B (yield 275) is closer on strength.
A204 Gr. BASTM / ASMENearYield 275 MPa, Rm 485–620 MPa, Mo 0.45–0.60.
A335 P1ASTM / ASMENearSeamless pipe: C 0.10–0.20, Mo 0.44–0.65, yield 205 MPa — the ASME C-½Mo pipe grade corresponding to 16Mo3 tube (EN 10216-2).
A182 F1ASTM / ASMENearC-½Mo forging grade (flanges, fittings).
15KhM / 16MGOST (Russia/CIS)NearGOST 20072 / 5520 grade 16M (Mo 0.25–0.35) is close; 15KhM adds Cr.
STPA12 / SB450MJIS (Japan)NearJIS G3462 STPA12 (0.5 Mo pipe) and G3103 SB450M (Mo boiler plate).
P265GHEN (European)FunctionalNon-alloy grade below 400–450 °C; 16Mo3 is the step up.
13CrMo4-5EN (European)Functional1.7335 Cr-Mo grade for 500–570 °C and hydrogen service.
P355GHEN (European)FunctionalMolybdenum-alloyed creep-resistant grade for service above 400 °C, where P355GH's guaranteed proof strength table ends.

Identical, near and functional are defined once on the grade index; the reason column below says which limit differs in each case.

16Mo3 in GB/T (China)

  • 16Mo — Identical GB/T 713 16Mo (formerly 16MnMoR-type usage); GB adopted the EN name for Mo pressure plate.

16Mo3 in ASTM / ASME

  • A204 Gr. A — Near ASTM/ASME A204 Grade A (SA-204-A): C ≤ 0.18, Mo 0.45–0.60, yield 255 MPa, Rm 450–585 MPa. Higher Mo than 16Mo3; Grade B (yield 275) is closer on strength.
  • A204 Gr. B — Near Yield 275 MPa, Rm 485–620 MPa, Mo 0.45–0.60.
  • A335 P1 — Near Seamless pipe: C 0.10–0.20, Mo 0.44–0.65, yield 205 MPa — the ASME C-½Mo pipe grade corresponding to 16Mo3 tube (EN 10216-2).
  • A182 F1 — Near C-½Mo forging grade (flanges, fittings).

16Mo3 in GOST (Russia/CIS)

  • 15KhM / 16M — Near GOST 20072 / 5520 grade 16M (Mo 0.25–0.35) is close; 15KhM adds Cr.

16Mo3 in JIS (Japan)

  • STPA12 / SB450M — Near JIS G3462 STPA12 (0.5 Mo pipe) and G3103 SB450M (Mo boiler plate).

16Mo3 in EN (European)

  • P265GH — Functional Non-alloy grade below 400–450 °C; 16Mo3 is the step up.
  • 13CrMo4-5 — Functional 1.7335 Cr-Mo grade for 500–570 °C and hydrogen service.
  • P355GH — Functional Molybdenum-alloyed creep-resistant grade for service above 400 °C, where P355GH's guaranteed proof strength table ends.

Superseded names for 16Mo3

  • 15Mo3 — DIN 17155 (withdrawn 1992): Same number 1.5415; still widely used name. Renamed 16Mo3 with the EN edition.
  • 16Mo3 — DIN 17175 (tubes)
  • 1503-243B / 1501-240 — BS 1501 / BS 3059: BS 3059 Part 2 grade 243 (tubes).
  • 15D3 — NF A 36-205

Key data for 16Mo3

Yield275 MPa ≤ 16 mm, +N
Tensile440–590 MPa
Carbon0.12 – 0.2 %
StandardEN 10028-2

Full composition, mechanical properties by thickness, heat treatment and applications for 16Mo3 →