Chemical Composition:
The chemical composition of A952/A952M-02(2016) steel grade is as follows:
– Carbon (C): 0.12% max
– Manganese (Mn): 0.60-1.00%
– Phosphorus (P): 0.04% max
– Sulfur (S): 0.05% max
– Silicon (Si): 0.15-0.40%
– Copper (Cu): 0.20% max
– Nickel (Ni): 0.40% max
– Chromium (Cr): 0.40% max
– Molybdenum (Mo): 0.15% max
Mechanical Properties:
The mechanical properties of A952/A952M-02(2016) steel grade are as follows:
– Tensile strength: 70-90 ksi (480-620 MPa)
– Yield strength: 50 ksi (345 MPa) min
– Elongation: 18% min
– Reduction of area: 35% min
– Hardness: Brinell 187 max
Standard Number:
The standard number for A952/A952M-02(2016) steel grade is ASTM A952/A952M-02(2016).
Corresponding Applications:
A952/A952M-02(2016) steel grade is commonly used in the manufacturing of structural components, such as beams, columns, and structural steel shapes. It can be found in construction, infrastructure, and engineering applications where high tensile strength and good weldability are required. The steel grade is also suitable for machining and can be used in various industries, including automotive, machinery, and equipment manufacturing.