Chemical Composition of A809-08(2017) Steel Grade:
The chemical composition of A809-08(2017) steel grade is as follows:
– Carbon (C): 0.08% max
– Manganese (Mn): 0.80-1.60%
– Phosphorus (P): 0.040% max
– Sulfur (S): 0.050% max
– Silicon (Si): 0.15-0.40%
– Nickel (Ni): 0.40% max
– Chromium (Cr): 0.40% max
– Copper (Cu): 0.35% max
Mechanical Properties of A809-08(2017) Steel Grade:
The mechanical properties of A809-08(2017) steel grade are as follows:
– Tensile Strength: 75 ksi (515 MPa) minimum
– Yield Strength: 55 ksi (380 MPa) minimum
– Elongation: 15% minimum
Standard number for A809-08(2017) Steel Grade:
A809-08(2017) is a standard specification for steel, plate, alloy, and high-strength, low-alloy, hot-rolled and cold-rolled for structural and commercial purposes. This standard is published by ASTM International.
Applications of A809-08(2017) Steel Grade:
A809-08(2017) steel grade finds its applications in various industries and purposes. It is commonly used in structural components and building construction due to its high strength and durability. It is also utilized in manufacturing heavy machinery, equipment, and vehicles. Additionally, A809-08(2017) steel grade is suitable for fabrication and welding processes, making it versatile for different engineering applications.